All concepts →A liquid metal is poured in a mold cavity of size 200 mm × 200 mm × 200 mm. The cooling is uniform in all directions with NO additional compensation for shrinkage. Considering the...
A liquid metal is poured in a mold cavity of size $200 \mathrm{~mm} \times 200 \mathrm{~mm} \times 200 \mathrm{~mm}$. The cooling is uniform in all directions with NO additional co...
Gray cast iron blocks of size $$100\,\,mm \times 50\,\,mm \times 10\,\,mm$$ with a central spherical cavity of diameter $$4$$ mm are sand cast. The shrinkage allowance for the patt...
A cubic casting of $$50mm$$ side undergoes volumetric solidification shrinkage and volumetric solid contraction of $$4\% $$ and $$6\% $$ respectively. No riser is used. Assume unif...
While cooling, a cubical casting of side $$40mm$$ undergoes $$3\% ,\,\,4\% $$ and $$5\% $$ volume shrinkage during the liquid state, phase transition and solid state respectively....
Gray cast iron blocks $$200 \times 100 \times 10\,\,mm$$ are to be cast in sand moulds. Shrinkage allowance for pattern making is $$1$$%. The ratio of the volume of pattern to that...
Which of the following materials requires the largest shrinkage allowance, while making a pattern for casting?
When there is no room temp change, the total shrinkage allowance on a pattern is INDEPENDENT OF